The Caking Reasons Of Caustic Soda Flakes

When using caustic soda, the user found that there are problems with caking that affect normal use, but it was not clear what caused this. Two possible causes of caustic soda clotting are summarized below.
1.Temperature of caustic Soda
The temperature of caustic soda is determined by the flow rate of cooling water and the rotating speed of machine. The amount of circulating water, the temperature circulating water, Whether the sprinkler is blocked and scale formation in the rotary drum of a caustic soda machine directly affect the temperature of caustic soda and the uniformity of the charging temperature of a caustic soda machine. After cleaning the sprinkler head,cleaning the scale formation,  increasing circulating water, decreasing the temperature of caustic soda flakes from 65℃ to 58℃, the caking phenomenon can be alleviated.

2.Caustic soda caking due to moisture Absorption
The laminar bag is a double-layer packing bag. If the seam is not fast enough or the seam is not tight enough, the laminar in the bag is easy to absorb moisture and affect its quality. So the original single seam was changed into a double seam, and the packaging personnel were required to inspect the processes of entrainment and suture, so as to achieve large air isolation and greatly reduce the problem of caking caused by loose sealing.
There is no direct relation between the quality and the caustic soda caking. However, if the caking happens, it will affect the normal use and the effect of use. Therefore, the manufacturer should pay special attention to the production and the use of users.
Marketing Center: Room 603, RuiYing Building, Chengnan 1st Road, Dali Town, Nanhai District, Foshan City, Guangdong Province,China, 528231
Factory: Area A No.9, Technology Park, Sanshui District, Foshan, Guangdong, China
Tel : +86 13929123248
Email : exp006@broviecn.com
Fax : 0086-0757-85510580

2019年9月25日星期三

Caustic Soda Manufacturer Tells You The Distinction Between Flake Alkali And Granular Alkali

Caustic soda is commonly known as sodium hydroxide, which is a basic chemical raw material. It is widely used in light industry such as papermaking, cotton fabric, chemical industry, machinery industry, metallurgy industry and so on. Many users will compare caustic soda flakes and caustic soda pearls, do not know the difference between the two, here is a summary of some relevant content.


The biggest difference between caustic soda flakes and caustic soda pearls is the shape, The caustic soda pearls are granular and caustic soda flakes are lamellar. In addition, the processing methods of caustic soda flakes and caustic soda pearls are also different. Granular caustic soda pearls is obtained by drying directly after production, while caustic soda flakes is obtained by pressing tablets. In application, pearls is easy to use and easy to weigh, which is mainly suitable for laboratory use. The cost of flakes is low, suitable for industrial production.


From the above, in addition to the different shapes of them, the application scope is different. Therefore, when choosing products, users only need to investigate the quality of good products according to their own industrial needs.

Marketing Center: RM 603, RuiYing Building, Nanhai District, Foshan, Guangdong, China
Factory : Area A No.9, Technology Park, Sanshui District, Foshan, Guangdong, China
Tel        : +86 13929123248
Email    : exp@broviecn.com
Fax       : 0086-757-85510580
Website : www.bv-alu.com